Definition and purpose
A die bonder (also called a die attach machine or die mounter) sits after wafer singulation and before interconnection. Finished wafers are usually mounted on dicing tape and a frame and diced, with the dies still in their array; the die bonder takes single dies off the tape, aligns them by vision, places them at the specified position on a lead frame, organic substrate, ceramic carrier or another die, and fixes them with a medium, forming a mechanical joint that survives later processes and, where required, an electrical or thermal path. [S1][S7]
Two boundaries that are easily confused must be drawn first. First, die attach and wire bonding are adjacent but different processes: the former bonds the die body to the carrier, and only the latter connects the die bond pads to the carrier leads with gold, aluminium or copper wire; writing them up as one machine or one mechanism leads to wrong materials, tools and inspection targets as well. [S1][S5]
Second, the attach medium is not a single route. The official ASMPT product matrix splits die bonding by medium and structure into Epoxy Die Bonding, Flip Chip Bonding, Multi-chip Module Bonding and Soft Solder Die Bonding, and separately lists the AD832U automatic eutectic die bonder and the SD8312 automatic soft solder die bonder; feeding, heating, atmosphere and post-cure conditions are not interchangeable between routes. [S1]
Mechanism and process chain
A typical placement starts on the supply side: the wafer table carries the diced wafer, ejector needles push the target die up from the back of the tape, and the pick tool (collet or nozzle) takes it by vacuum; machine vision recognizes the die outline and orientation, and the bond head places the die at the compensated coordinates on a carrier already prepared with medium, applies the set force, temperature and dwell, and then the part goes to curing or reflow. The ASMPT AD830 Plus model page states that it uses dual decoupled linear-motor bond heads, dual stamping/dispensing, a rotary collet bond arm, automatic theta capture during pick and place, and static bond optics for pre- and post-bond inspection. [S2]
The epoxy route meters adhesive onto the carrier by dispensing or stamping, then cures it by heat. Henkel LOCTITE ABLESTIK 84-1LMISR4 is a one-part silver-filled conductive epoxy die attach adhesive; its official product page gives a cure of 1 hour at 175°C and notes that its rheology suits high-speed automated equipment and reduces tailing during dispensing and die placement dwell. [S8] Such values are typical material values, not an equipment process window.
The conductive die attach film (DAF) route laminates the medium to the wafer back beforehand; after dicing the film is picked up with the die and bonded with heat and pressure at placement, removing per-die dispensing. The technical data sheet for Henkel LOCTITE ABLESTIK CDF 900 gives the conditions in detail: PSA dicing tape as carrier, tape 85 µm, adhesive layer in 15 µm and 30 µm versions, for 8-inch and 12-inch wafers; wafer backside lamination at 70°C, 20–40 psi, 1–4 ft/min; die attach at 90–110°C, 0.5–1 kg, 0.5–1 seconds; recommended cure ramping from 25°C to 175°C in 30 minutes and holding 60 minutes (pressure oven at 7 kg/cm²). [S7] These conditions apply only to that product and are not extrapolated to other DAF products.
Eutectic, soft solder and thermocompression bonding form another group of mechanisms. The official ASMPT AMICRA NOVA page lists diode laser, hot-plate eutectic or epoxy stamping/dispensing as options on the same platform and states that it holds placement accuracy at ±1.0 µm @ 3 s at over 350°C and high bond force, classing such configurations as thermocompression bonding (TCB) or TSV applications. [S3] When K&S launched the APAMA in 2014 it positioned it as a chip-to-substrate thermocompression bonder covering NCF (non-conductive film), NCP (non-conductive paste) and TC CUF (thermocompression capillary underfill), stressing a direct-drive Z-axis bond head, on-machine metrology and programmable ramp rates. [S5] Heating with pressure is only a shared appearance; the material form and interface formation mechanisms differ.
Parameters with model-level conditions
Throughput must be read with its conditions. The official ASMPT AD830 Plus page says up to 22,000 UPH, and the same page's footnote states explicitly that all performance is package and material dependent; it is the model's upper limit with suitable package and material and cannot serve as a general cycle rate for the whole category. [S2] When K&S launched the iStack PS platform in 2009 it said up to 30% more throughput than its previous-generation die bonders of the time; that is a historical maker statement against a stated baseline and likewise not a specification for current machines. [S4]
Placement accuracy must also be separated by model and cycle time. The official ASMPT AMICRA NOVA page gives ±1.0 µm @ 3 s, a cycle time under 3 seconds and a substrate work area of 550×600 mm, and lists automatic loading of 12-inch/300 mm wafers and 450 mm substrate wafers; the same page lists the AMICRA NANO at ±0.2 µm @ 3 s and the CoS model at ±1.5 µm with a cycle under 15 seconds. [S3] Three figures from three models cannot be merged into one die bonder accuracy.
An ASM AD830 registered on the Nanjing University of Science and Technology large instrument sharing platform (instrument number 20234527, purchased 2023-01-14) gives machine figures that can be compared directly: cycle time 160 msec, positioning accuracy ±1.5 mil, angular accuracy ±3°, die size 6 mil×6 mil to 100 mil×100 mil, bond force 20–200 g, travel 8″×8″ (203 mm×203 mm), repeatability ±0.2 mil, ejector stroke 3 mm. [S10] These are a university platform's registered values for one specific machine, not an official ASMPT specification; this entry does not convert or equate them with 22,000 UPH, as the two sources differ in nature and basis.
Typical material values form a separate column. The official Henkel ABLESTIK 84-1LMISR4 page lists viscosity 8000 mPa·s (Brookfield CP51 @ 25°C), thermal conductivity 2.5 W/mK, volume resistivity ≤0.0002 Ω·cm, glass transition temperature 120°C, CTE 40 ppm/°C (150 ppm/°C above Tg), moisture absorption 0.6% after 168 hours at 85°C/85%RH and tensile modulus 300 N/mm² at 250°C. [S8] ABLESTIK 2100A targets lead-free PBGA/BGA; its official page says it withstands 500°F (260°C) reflow, suits dies up to 12.7 mm×12.7 mm, has CTE 65 ppm/°C, and typical die shear strength of 16.0 kg-f at room temperature and 5.0 kg-f hot. [S9] These are typical performance data from material pages, not equipment parameters, and they are not acceptance criteria.
Variants
By medium and structure, the official ASMPT product matrix divides die bonding into epoxy die bonding, flip chip bonding, multi-chip module bonding and soft solder die bonding, and lists the AD832U automatic eutectic die bonder and SD8312 automatic soft solder die bonder separately among related products; at equipment level eutectic and soft solder are thus separate machine types, not the same machine with a different program. [S1]
By wafer size and degree of automation, the same matrix lists the AD8312Plus series for 12-inch wafers, the AD832i for 8-inch wafers and the AD8312FC flip-chip model; a 2018 K&S trade-show announcement positioned the iStack W+ for thinner dies and substrates and offering wafer-level placement. [S1][S6]
By accuracy and purpose, besides high-volume automatic die bonders there are high-accuracy and ultra-high-accuracy platforms. The AMICRA NOVA targets advanced packaging, MEMS, automotive sensors, optoelectronics and silicon photonics, supporting multi-die, wafer mapping, post-bond inspection and active bond force control; the same maker's NANO is headlined at ±0.2 µm @ 3 s. [S3] These are positioned differently from high-throughput models such as the AD830 Plus, and their figures cannot be applied to each other when selecting. [S2]
Selection and design
Settle the medium route first, then the machine. Conductive adhesive calls for dispensing or stamping plus oven curing; DAF calls for wafer backside lamination, dicing tape and placement heating and pressure (CDF 900's lamination at 70°C, 20–40 psi and placement at 90–110°C, 0.5–1 kg are product-level examples); eutectic or soft solder needs the corresponding dedicated machine and heating method. [S7][S1][S3]
Read three kinds of figures separately: equipment capability (UPH, cycle time), positioning or placement accuracy (µm or mil, with cycle time conditions), and typical material properties (viscosity, thermal conductivity, shear strength). The AD830 Plus 22,000 UPH carries a package-and-material footnote, the AMICRA NOVA ±1.0 µm carries a 3-second cycle condition, and the NJUST AD830's ±1.5 mil is a registered value; merging them into one die bonder parameter table misleads selection. [S2][S3][S10]
Check whether pick, place and inspection form a closed loop. The AD830 Plus uses a rotary collet bond arm, automatic theta capture during pick and place, and static bond optics for pre- and post-bond inspection; the APAMA stresses on-machine overlay metrology and process drift detection; the AMICRA NOVA offers wafer mapping, post-bond inspection and metrology, and active bond force control. These are different makers' answers to how placement accuracy is assured, to be weighed against product requirements. [S2][S5][S3]
Check material and downstream processes together. The official 2100A page states it is a PBGA/BGA adhesive withstanding 260°C lead-free reflow; the CDF 900 cure profile includes a 60-minute hold at 175°C; if wire bonding and molding follow, temperature history, interface voids and ionic content must be checked against the material page conditions. [S9][S7] The public material available gives no first-hand specification for die bonder cleanliness class or ESD conditions, so no general values are given here; specific conditions must still be confirmed against the applicable specification.
FAQ
Q: Are a die bonder and a wire bonder the same machine? A: No. Die attach fixes the die to the carrier, and wire bonding then connects the die bond pads to the carrier leads with metal wire; the ASMPT product matrix lists Die Bonding and Wire Bonding as separate process categories. [S1]
Q: Can silver epoxy, DAF and eutectic be swapped just by changing the program? A: Not in general. Their feeding, lamination or dispensing modules, and heating and curing conditions all differ; CDF 900 needs wafer backside lamination with matching dicing tape, 84-1LMISR4 is a dispensed one-part adhesive, and eutectic bonding on the AMICRA NOVA can use a diode laser or hot plate. [S7][S8][S3]
Q: Can every package reach 22,000 UPH? A: No. ASMPT's footnote on the AD830 Plus page states that all performance depends on package and material; the value is the model's upper limit, not a general cycle rate. [S2]
Q: Is ±1 µm the general accuracy of die bonders? A: No. That is the official AMICRA NOVA value at a 3-second cycle; the same maker's NANO and CoS models give other figures, and the university-registered AD830 uses mil. [S3][S10]
Q: Can the die shear strength on a material page be used directly as an acceptance criterion? A: Not advisable. The 2100A and CDF 900 figures are typical material performance data; die attach strength testing has its own methods, and the public material available does not include the full text of standards bodies' methods, so no specific criteria, failure classifications or sampling requirements are given here; specific conditions must still be confirmed against the applicable specification. [S9][S7]
Upstream, downstream and standards boundary
Upstream are wafer thinning, tape mounting and dicing (singulated dies stay on the tape), lead frames, substrates or carriers, and the attach materials and supply system; downstream are wire bonding, molding, lead-free reflow and reliability testing. 2100A is designed explicitly for 260°C lead-free reflow, showing that die attach material choice must follow the downstream temperature history. [S9]
The standards boundary is stated as it is: the ASMPT, K&S and Henkel pages are maker materials, not standard texts, and die shear strength on a material page is a typical material property. Die attach strength and wire pull address different failure objects; the public material available does not include the full text of standards bodies' methods, so no method numbers, criteria or sample sizes are given and no standard version is ruled on. [S8][S9]
The wire-bonder entry in the same batch already covers wire bonding mechanisms along the ball and wedge routes; this entry covers die attach only. The two are each other's upstream and downstream, and their citations are not used in place of each other. [S1]
Functional modules
Wafer table and ejector
Carries the diced wafer for expansion, locating and ejecting single dies. Ejector needles push the target die off the back of the dicing tape for the pick tool; the AD830 registered at NJUST has an ejector stroke of 3 mm and a die size range of 6 mil×6 mil to 100 mil×100 mil, values registered for that machine. [S10]
Pick-and-place bond head
Performs vacuum pick-up, angle compensation, alignment, placement pressure and dwell. The AD830 Plus uses dual decoupled linear-motor bond heads and a rotary collet bond arm with automatic theta capture during pick and place; the AMICRA NOVA adds active bond force control. [S2][S3]
Attach-medium dispensing
Configured by route for dispensing, stamping, DAF lamination or solder supply. The AD830 Plus page lists dual stamping/dispensing; 84-1LMISR4 is a dispensed one-part silver-filled epoxy; CDF 900 is supplied as conductive film pre-laminated to the wafer back, laminated at 70°C and 20–40 psi. [S2][S8][S7]
Heating and curing
Provides bond head and stage heating and post-cure conditions. CDF 900 is placed at 90–110°C for 0.5–1 second with a recommended cure of 60 minutes at 175°C; 84-1LMISR4 cures 1 hour at 175°C; the AMICRA NOVA can do eutectic bonding by diode laser or hot plate, and its page mentions bonding conditions above 350°C. [S7][S8][S3]
Vision and alignment
Recognizes die outline and orientation, corrects carrier position and inspects before and after placement. The AD830 Plus uses static bond optics to capture pre- and post-bond images; the APAMA stresses on-machine overlay metrology and process drift detection; the AMICRA NOVA offers wafer mapping and post-bond inspection and metrology. [S2][S5][S3]
Substrate handling
Conveys lead frames, substrates or carriers and handles locating, loading and unloading. The official AMICRA NOVA page gives a substrate work area of 550×600 mm and lists automatic loading of 12-inch/300 mm wafers and 450 mm substrate wafers; the AD8312Plus and AD832i handle 12-inch and 8-inch wafers respectively. [S3][S1]
Control, recipe and traceability
Manages recipes, force and temperature profiles, throughput statistics and process data. In the APAMA launch release K&S stressed portable recipes and integrated metrology and analytics for advanced process control; the iStack PS was positioned at its 2009 launch for stacked die and high-performance BGA applications. [S5][S4]
Manufacturer & technical sources
Continue with manufacturer product pages, operating principles and technical information for this equipment type.